Filament Drying  @Circadea






Esun
Filament Containers



Bartelli System

 




Probably the easiest and most common way of drying filament is
throwing it in the oven.
Just set the temperature to right below the glass transition
temperature of the plastic,
and leave it in there for 4-6 hours for the moisture to cook out.
The longer you leave it, the more drying you’ll get.


Drying Times PLA 45°C (113°F) - 4h ABS 60°C (140°F) - 2h PETG 65°C (149°F) - 2h Nylon 70°C (158°F) - 12h Silic 65°C (149°F) - 3h PVA 45°C (113°F) - 4h TPU/TPE 50°C (122°F) - 4h

Timer
Video using a food dehydrator.


Thermometer

Printdry